Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ISO 2781
Maximum Moisture Content 0.050
0.050
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ISO 868
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ISO 37
Elongation at Break 580 %
580 %
ISO 37
Tensile Modulus 0.0430 GPa
6.24 ksi
ISO 527
50% Modulus 0.00750 GPa
1.09 ksi
ISO 37
100% Modulus 0.00950 GPa
1.38 ksi
ISO 37
300% Modulus 0.0200 GPa
2.90 ksi
ISO 37
Rebound 45 %
45 %
ISO 4662
Tear Strength 95.0 kN/m
542 pli
with incision; ISO 34B
133 kN/m
759 pli
without incision; ISO 34B
Abrasion 25
25
mm<sup>3</sup>; ISO 4649
Compression Set 17 %
17 %
70 hrs./22°C; ISO 815
33 %
33 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
A50; ISO 306
Processing Properties Metric English Comments
Zone 1 190 °C
374 °F
Extrusion
Zone 2 195 °C
383 °F
Extrusion
Zone 3 200 °C
392 °F
Extrusion
Zone 4 200 °C
392 °F
Extrusion
Adapter Temperature 200 °C
392 °F
5, Extrusion
Die Temperature 195 °C
383 °F
6, Extrusion
195 °C
383 °F
Tip, 7, Extrusion
Drying Temperature 100 °C
212 °F
Dry Time 3.00 hour
3.00 hour
Dew Point >= -30.0 °C
>= -22.0 °F
Copyright © lookpolymers.com All Rights Reserved