Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Dryflex® 9012-001 TPE, Modified Injection Molding Grade for Semi Rigid Molding

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 9012-001 TPE, Modified Injection Molding Grade for Semi Rigid Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 9012-001 is specifically designed for semi-rigid moldings.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 2781
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ISO 868
Tensile Strength at Break 14.5 MPa
2100 psi
ISO 37
Elongation at Break 900 %
900 %
ISO 37
100% Modulus 0.00950 GPa
1.38 ksi
ISO 37