Mechanical Properties Metric English Comments
100% Modulus 0.00720 GPa
1.04 ksi
-10% change after 72 hours @ 260°C; ASTM D412
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer
Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur..
100% Modulus 0.00720 GPa
1.04 ksi
DIN 53504
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
100% Modulus 0.00720 GPa
1.04 ksi
ASTM D412
DuPont Vamac® DP Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00720 GPa
1.04 ksi
ASTM D412
DuPont Performance Polymers Kalrez® 6375UP FFKM Perfluoroelastomer
Resists chemical attack and is formulated and processed to minimize the potential for undesirable contaminants. Kalrez® 6375UP has the best balance of performance characteristics required for semic..
100% Modulus 0.00720 GPa
1.04 ksi
500 mm/min; ASTM D412
DuPont Performance Polymers Kalrez® 6375 FFKM Perfluoroelastomer
Kalrez Spectrum 6375, designed specifically for the chemical process industry, combines new polymer technology with innovative patented curing technology. Compound 6375 is designed to give outstandi..
100% Modulus 0.00717 GPa
1.04 ksi
ASTM D-638
Axiall 801-83 Moldings & Extrusions Flexible PVC
High temperature automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00720 GPa
1.04 ksi
ASTM D412
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer
A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen..