100% Modulus 0.00717 GPa
1.04 ksi
ASTM D-638
Axiall 801-83 Moldings & Extrusions Flexible PVC
High temperature automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.