Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00538 GPa
0.781 ksi
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.00538 GPa
0.781 ksi
DCBP Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..