Polymer Property : 100% Modulus = 0.00538 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00538 GPa
0.781 ksi
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
100% Modulus 0.00538 GPa
0.781 ksi
DCBP Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..
100% Modulus 0.00538 GPa
0.780 ksi
ASTM D412
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.00538 GPa
0.780 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00538 GPa
0.780 ksi
Press Cure 15 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FLS 2650 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FLS 2650 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..