Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 88
84 - 88
Tensile Strength 24.5 MPa
3560 psi
Elongation at Break 650 %
650 %
100% Modulus 0.00538 GPa
0.781 ksi
300% Modulus 0.00981 GPa
1.42 ksi
Processing Properties Metric English Comments
Processing Temperature 175 - 200 °C
347 - 392 °F