Mechanical Properties Metric English Comments
100% Modulus 0.00514 GPa
0.745 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188; DIN 53508
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber
Information provided by Advanced Polymer Alloys
100% Modulus 0.00514 GPa
0.745 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2260 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2260 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..