Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ FC 2260 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FC 2260 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dyneon™ Fluoroelastomer FC 2260 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2260 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Composition: di-polymer of vinylidene fluoride and hexafluoropropylene plus cure site monomerCan be used in blends with fluorosilicone, silicone, EDPM and other peroxide curable elastomersProcess targets: transfer and compression molding and calenderingPeroxide cure technologySlightly improved water and steam resistance over conventional fluoroelastomerVulcanization of thick cross-section parts without fissuringInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 60

@Temperature 121 °C
60

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 16.17 MPa
2345 psi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 225 %
225 %
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00514 GPa
0.745 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 25 %
25 %
Aged 70 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Translucent to Off-White
MH, Maximum Torque 11.1 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque 2.1 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Solubility Partially soluble in low molecular weight esters and ketones
t`50, Time to 50% cure 1.1 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 3 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 0.8 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C
Copyright © lookpolymers.com All Rights Reserved