Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00514 GPa | 0.745 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188; DIN 53508 |
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
100% Modulus | 0.00514 GPa | 0.745 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2260 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2260 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |