Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00460 GPa | 0.667 ksi | DIN 53504 |
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | DIN 53504 |
Lubrizol ESTANE® T5384 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | ISO 37 |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | |
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | DIN 53504 |
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58201 Thermoplastic Polyurethane Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.Features: Tear resistant properties.Uses: Injection Molding and general extrusion techniques.Available in Euro.. |
|||
100% Modulus | 0.00460 GPa | 0.667 ksi | ISO 37 |
AlphaGary Evoprene™ 042 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |