Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: High resilient, low temperature flexibility Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ISO 37
Elongation at Break 810 %
810 %
ISO 37
Tensile Modulus 0.0120 GPa
1.74 ksi
ISO 527
50% Modulus 0.00350 GPa
0.508 ksi
ISO 37
100% Modulus 0.00460 GPa
0.667 ksi
ISO 37
300% Modulus 0.00660 GPa
0.957 ksi
ISO 37
Rebound 56 %
56 %
ISO 4662
Tear Strength 35.0 kN/m
200 pli
with incision; ISO 34B
Abrasion 90
90
mm<sup>3</sup>; ISO 4649
Compression Set 21 %
21 %
70 hrs./22°C; ISO 815
65 %
65 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 56.0 °C
133 °F
A50; DIN 53460
Brittleness Temperature -70.0 °C
-94.0 °F
DIN 53546