Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00296 GPa | 0.430 ksi | |
Spartech E65050 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00296 GPa | 0.430 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00296 GPa | 0.430 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
100% Modulus | 0.00296 GPa | 0.430 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00296 GPa | 0.430 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |