Spartech E65050 General Purpose PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech E65050 General Purpose PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for clear tubing, profiles, co-extrusion.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
+.02
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
10 sec ± 3
Tensile Strength, Yield 8.27 MPa
1200 psi
Elongation at Break 498 %
498 %
100% Modulus 0.00296 GPa
0.430 ksi
Processing Properties Metric English Comments
Melt Temperature 149 °C
300 °F