100% Modulus 0.00296 GPa
0.429 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-270A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00296 GPa
0.430 ksi
Spartech E65050 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00296 GPa
0.430 ksi
ASTM D412
Teknor Apex UNIPRENE® 7100-64 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00296 GPa
0.430 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui..
100% Modulus 0.00296 GPa
0.430 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 2060 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00296 GPa
0.430 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 4660 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..