Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.178 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00123 GPa
0.178 ksi
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer
KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to..
100% Modulus 0.00123 GPa
0.178 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer
Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited..
100% Modulus 0.00123 GPa
0.178 ksi
ASTM D412
Advanced Polymer Alloys DuraGrip™ 6140 TR Thermoplastic Elastomer
DuraGrip® DGR6140TR is a translucent thermoplastic elastomer formulated for excellent elastic properties and enhanced adhesion to various engineered thermoplastics using insert molding, co-injectio..
Copyright © lookpolymers.com All Rights Reserved