Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00123 GPa | 0.178 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to.. |
|||
100% Modulus | 0.00123 GPa | 0.178 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
100% Modulus | 0.00123 GPa | 0.178 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6140 TR Thermoplastic Elastomer DuraGrip® DGR6140TR is a translucent thermoplastic elastomer formulated for excellent elastic properties and enhanced adhesion to various engineered thermoplastics using insert molding, co-injectio.. |