Total HP 401N Natural HDPE, pipe

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HP 401N Natural HDPE, pipe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
No failures; ASTM D1693 cond. C 100% lgepal
Melt Flow 0.080 g/10 min

@Load 2.16 kg
0.080 g/10 min

@Load 4.76 lb
ASTM D 1238
0.34 g/10 min

@Load 5.00 kg
0.34 g/10 min

@Load 11.0 lb
ASTM D 1238
High Load Melt Index 7.0 g/10 min

@Load 21.6 kg
7.0 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
PENT >= 100 hour
>= 100 hour
ASTM F 1473
Hardness, Shore D 63
63
ASTM D 2240
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D 638 type IV
Elongation at Break >= 800 %
>= 800 %
ASTM D 638 type IV
Flexural Modulus 0.862 GPa
125 ksi
ASTM D 790
Izod Impact, Notched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Hydrostatic Design Basis 11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D 2837
Thermal Properties Metric English Comments
Melting Point 126 °C
258 °F
ASTM D3417