Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 12.0 J @Temperature -40.0 °C |
8.85 ft-lb @Temperature -40.0 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Impact Test | 12.0 J @Temperature -30.0 °C |
8.85 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Impact Test | 12.0 J @Thickness 4.00 mm |
8.85 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Impact Test | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 12.0 J @Temperature 100 °C |
8.85 ft-lb @Temperature 212 °F |
Charpy-V specimens, transverse direction. |
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Impact Test | 12.0 J @Thickness 4.00 mm |
8.85 ft-lb @Thickness 0.157 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Impact Test | 12.0 J @Thickness 4.00 mm |
8.85 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 12.0 J @Temperature 23.0 °C |
8.85 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66 Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |