Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 82.0 J @Temperature 23.0 °C |
60.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Impact Test | 82.0 J @Temperature 23.0 °C |
60.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Impact Test | 82.0 J @Temperature 23.0 °C |
60.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Impact Test | 82.0 J @Temperature 23.0 °C |
60.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 82.0 J @Temperature -40.0 °C |
60.5 ft-lb @Temperature -40.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Impact Test | 82.0 J @Thickness 3.17 mm, Temperature -40.0 °C |
60.5 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM |
Braskem ML3601U LLDPE Rotomolding Polyethylene The resin ML3601U is a linear low-density polyethylene, 1-hexene based, with excellent environmental stress cracking resistance and high impact strength. It contains long term UV8 stabilization and .. |