Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Instrumented, 2.2 m/s, ductile; ASTM D3763 |
Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued .. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Impact Test | 24.0 J @Temperature -18.0 °C |
17.7 ft-lb @Temperature -0.400 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Impact Test | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Multiaxial Impact; E-max; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |