Mechanical Properties Metric English Comments
Impact Test 21.7 J

@Temperature -40.0 °C
16.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin  (discontinued **)
OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and..
Impact Test 21.7 J

@Temperature 23.0 °C
16.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil ESCOR™ AT 325 Molding, extrusion and compounding resin  (discontinued **)
ESCOR AT 325 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials. It has the highest melt index and the lowest modulus of all the Escor Acid Terpoly..
Impact Test 21.7 J

@Temperature 23.0 °C
16.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..