Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 21.7 J @Temperature -40.0 °C |
16.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |
|||
Impact Test | 21.7 J @Temperature 23.0 °C |
16.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil ESCOR™ AT 325 Molding, extrusion and compounding resin
(discontinued **) ESCOR AT 325 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials. It has the highest melt index and the lowest modulus of all the Escor Acid Terpoly.. |
|||
Impact Test | 21.7 J @Temperature 23.0 °C |
16.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |