Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Poco Graphite EDM-200 EDM Graphite POCO's EDM-200 is an isotropic Superfine particle graphite providing good strength, surface finish, and wear resistance.Applications:Structural ribsRoughing or finishing electrodesLarge featured mol.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Ohio Carbon Blank OCB EDM-200 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-205 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0230 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polycarbonate for Injection Molding 10% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0080 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 110 MPa | 14000 - 16000 psi | ASTM D695 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Compressive Strength | 96.5 - 103 MPa | 14000 - 15000 psi | ASTM D695 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Transverse; ASTM D-695 |
Glastic SG-200 Corner Angles Corner angles used for coil winding.Information provided by Glastic Corporation |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Techmer ES Luriblend® PA6 E M/SL4 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant and Silicone LubricantFeatures: Low Friction, Good Wear Resistance and LubricatedAppearance: BlackInformation provid.. |
|||
Compressive Strength | >= 96.5 MPa | >= 14000 psi | |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | cured |
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value .. |
|||
Compressive Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Ultimate; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |