Polymer Property : Compressive Strength = 950 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 950 MPa
138000 psi
Chemically Strengthened to 40 µm Depth
Corning Gorilla® Glass 3 Touch Screen Glass with NDR
Gorilla® Glass 3 with Native Damage Resistance™ (NDR) is an alkali-aluminosilicate thin sheet glass that is better able to survive the real-world events that most commonly cause glass failure. Wit..