Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 950 MPa | 138000 psi | Chemically Strengthened to 40 µm Depth |
Corning Gorilla® Glass 3 Touch Screen Glass with NDR Gorilla® Glass 3 with Native Damage Resistance™ (NDR) is an alkali-aluminosilicate thin sheet glass that is better able to survive the real-world events that most commonly cause glass failure. Wit.. |