Polymer Property : Compressive Strength = 62.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated  (discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Compressive Strength 62.1 MPa
9010 psi
Henkel Hysol EA 9321 Paste Adhesive System
Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/13/SI/2 BK3585 Polycarbonate
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/13/SI/2 NAT Polycarbonate
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/15 NAT Polycarbonate
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/22 BK223 Polycarbonate
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/22 NAT Polycarbonate
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/13/SI/2 WT8966 Polycarbonate
Compressive Strength >= 62.1 MPa
>= 9000 psi
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications
Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate..
Compressive Strength 62.1 MPa
9000 psi
Service Pressure
Trelleborg AEM Eccofloat® EL-34/6000 Syntactic Foam
EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydr..
Compressive Strength 62.1 MPa
9000 psi
ASTM D790
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste
BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid
Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid
Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste
Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste
Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond ..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste
SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common..
Compressive Strength 62.1 MPa
9000 psi
3M Scotchkote™ FG 502 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha..
Compressive Strength 62.1 MPa
9000 psi
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina
Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required.
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste
BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid
Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste
SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra..
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid
Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn..
Compressive Strength 62.1 MPa
9010 psi
Henkel Hysol EA 9313 Paste Adhesive System
Very low viscosity adhesive yielding tough, flexible bonds. Injectable.
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Techmer ES Plaslube® PC-50/TF/15 BK223 Polycarbonate