Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® PC-50/TF/22 NAT Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, PTFE Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® PC-50/TF/22 NAT Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 0.12 %
0.12 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength at Break 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Compressive Strength 62.1 MPa
9000 psi
ASTM D695
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C

@Temperature 20.0 °C
39.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Users viewing this material also viewed the following: