Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0400 MPa | 5.80 psi | 25% deformation |
Unifrax Fiberfrax® 970 Ceramic Fiber Paper 970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. .. |