Compressive Strength 0.0400 MPa
5.80 psi
25% deformation
Unifrax Fiberfrax® 970 Ceramic Fiber Paper
970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. ..