Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 5.50 MPa @Time 3.60e+7 sec |
798 psi @Time 10000 hour |
|
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Compressive Strength | 5.50 - 7.50 MPa @Temperature 23.0 °C, Time 86400 sec |
798 - 1090 psi @Temperature 73.4 °F, Time 24.0 hour |
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |