Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 5.50 - 7.50 MPa @Temperature 23.0 °C, Time 86400 sec |
798 - 1090 psi @Temperature 73.4 °F, Time 24.0 hour |
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |