Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified

Category Polymer , Thermoplastic
Manufacturer Wolf Kunststoff
Trade Name ZEDEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided by Zedex
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.65 %
0.65 %
DIN EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore A >= 100
>= 100
DIN 53505
Hardness, Shore D 56
56
DIN 53505
Ball Indentation Hardness 49.0 MPa
7110 psi
DIN 2039
Tensile Strength at Break 30.0 MPa
4350 psi
DIN EN ISO 527
Tensile Strength 37.0 MPa
5370 psi
DIN EN ISO 527
Tensile Stress 4.00 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
580 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Tensile Strength, Yield 4.00 MPa
580 psi
Elastic Limit
14.0 MPa
2030 psi
DIN EN ISO 527
Elongation at Break >= 300 %
>= 300 %
DIN EN ISO 527
Elongation at Yield 2.0 %
2.0 %
Elastic Yield Point
9.0 %
9.0 %
Flexural; DIN EN ISO 178
20 %
20 %
DIN EN ISO 527
Tensile Modulus 0.200 GPa
29.0 ksi
DIN EN ISO 527
Flexural Strength 11.0 MPa
1600 psi
Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
17.0 MPa
2470 psi
DIN EN ISO 178
Flexural Modulus 0.350 GPa
50.8 ksi
DIN EN ISO 178
Compressive Strength 14.0 MPa
2030 psi
Elastic Limit
5.50 MPa

@Time 3.60e+7 sec
798 psi

@Time 10000 hour
12.0 MPa

@Time 360000 sec
1740 psi

@Time 100 hour
15.0 MPa

@Time 36.0 sec
2180 psi

@Time 0.0100 hour
6.00 MPa

@Strain 3.50 %
870 psi

@Strain 3.50 %
DIN EN ISO 604
Compressive Modulus 0.334 GPa
48.4 ksi
DIN EN ISO 604
Fatigue Strength 7.00 MPa

@# of Cycles 1.00e+6
1020 psi

@# of Cycles 1.00e+6
1 Hz
K Factor (ISO) 2.3 µm/km

@Temperature 100 °C
2.3 µm/km

@Temperature 212 °F
5.4 µm/km

@Temperature 20.0 °C
5.4 µm/km

@Temperature 68.0 °F
Charpy Impact Unnotched NB
NB
EN ISO 179/1eU
Charpy Impact, Notched NB
NB
EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.080

@Temperature 100 °C
0.080

@Temperature 212 °F
Dry Operation
0.80

@Temperature 20.0 °C
0.80

@Temperature 68.0 °F
Dry Operation
Coefficient of Friction, Static 0.25

@Temperature 20.0 °C
0.25

@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 400 MPa
58000 psi
At 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.0140 MPa-m/sec
400 psi-ft/min
v = 1m/min
0.02833 MPa-m/sec
808.8 psi-ft/min
v = 10m/min
Compression Set 7.1 %
7.1 %
Elastic Compression Limit
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C

@Temperature <=150 °C
90.0 µin/in-°F

@Temperature <=302 °F
ISO E 831
168 µm/m-°C

@Temperature <=100 °C
93.3 µin/in-°F

@Temperature <=212 °F
ISO E 830
Specific Heat Capacity 1.75 J/g-°C
0.418 BTU/lb-°F
DSC
Melting Point 207 °C
405 °F
DSC
Maximum Service Temperature, Air 50.0 °C
122 °F
Pressed Bushings
75.0 °C
167 °F
Continuous
80.0 °C
176 °F
Short Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
DIN EN ISO 75
Glass Transition Temp, Tg -64.0 °C
-83.2 °F
DSC
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
IEC 93
Surface Resistance 4.00e+12 ohm
4.00e+12 ohm
IEC 93
Dielectric Constant 4.4

@Frequency 110 Hz
4.4

@Frequency 110 Hz
IEC 250
Dielectric Strength 21.0 kV/mm
533 kV/in
IEC 243
Dissipation Factor 0.011
0.011
IEC 112
0.141

@Frequency 1.00 Hz
0.141

@Frequency 1.00 Hz
Descriptive Properties Value Comments
Alignment Adjustment 10
Nominal Scale: 1, low; 10, high
Color Black
Creep Resistance 2
Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion 2
Nominal Scale: 1, low; 10, high
FDA Compliant Applicable
Free from PTFE Applicable
Free from Silicon Applicable
Gamma-rays Radiation Sterilization 3
Nominal Scale: 1, low; 10, high
High Precision Bushings (negative clearance) Applicable
Injection Molded Parts Applicable
Machined Parts Applicable
Moist Heat Sterilization 6
Nominal Scale: 1, low; 10, high
Plastic Granules Applicable
Resistance Against dust, Dirt, Abrasive Substances 8
Nominal Scale: 1, low; 10, high
Resistance Against Hot Water 70
Resistance to Chemicals 5
Nominal Scale: 1, low; 10, high
Rods up to Øe (de) Applicable
Sheets up to Maximum Thickness Applicable
Sliding Velocity 10
Suitable for Outdoor Use 7
Nominal Scale: 1, low; 10, high
Suitable for Use in Water Applicable
Suitable for Vacuum Applicable
Tubes (hollow rods) up to Øe (de) Applicable
UV Rays Resistance 8
Nominal Scale: 1, low; 10, high
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved