Polymer Property : Compressive Strength = 435 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 3.00 MPa
435 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica PE 1000 - Polyethylene 1000
Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there..
Compressive Strength 3.00 MPa
435 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica PE 300 - Polyethylene 300
Molecular weight 300,000 polyethylene similar to the type 500 with higher rigidity and lower resistance to continuous shocks. The applications are similar to those of PE 500, being more commonly spe..
Compressive Strength 3.00 MPa
435 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica PE 500 - Polyethylene 500
Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff..
Compressive Strength 3.00 MPa
435 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica PVDF Kynar
PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe..
Compressive Strength 3.00 MPa
435 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Compressive Strength 3.00 MPa
435 psi
In the Foaming Direction
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..
Compressive Strength 3.00 MPa
435 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZ-3000 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 3.00 MPa

@Temperature 23.0 °C
435 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto