Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 280 - 330 MPa | 40600 - 47900 psi | ISO 604 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Compressive Strength | 280 MPa | 40600 psi | ASTM D695 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Compressive Strength | 280 MPa | 40600 psi | ISO 604 |
Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
Compressive Strength | 280 MPa | 40600 psi | ISO 604 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Compressive Strength | 280 MPa @Thickness >=5.00 mm |
40600 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera.. |
|||
Compressive Strength | 280 MPa @Thickness >=5.00 mm |
40600 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g.. |
|||
Compressive Strength | 280 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
40600 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |