Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 280 - 330 MPa | 40600 - 47900 psi | ISO 604 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Compressive Strength | 270 - 330 MPa | 39200 - 47900 psi | ISO 604 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |