Compressive Strength 259 MPa
37500 psi
SGL Carbon Group EK 3205 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..