Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.70 MPa | 247 psi | perpendicular to plane; ASTM D1621 |
SABIC Innovative Plastics ULTEM Foam XP110 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Compressive Strength | >= 1.70 MPa | >= 247 psi | perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Compressive Strength | 1.70 MPa | 247 psi | to 30% deformation with density of 0.320 g/cc |
Pyrotek MT-29B Microporous Insulating Board MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T.. |