Mechanical Properties Metric English Comments
Compressive Strength 1.70 MPa
247 psi
perpendicular to plane; ASTM D1621
SABIC Innovative Plastics ULTEM Foam XP110 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Compressive Strength >= 1.70 MPa
>= 247 psi
perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Compressive Strength 1.70 MPa
247 psi
to 30% deformation with density of 0.320 g/cc
Pyrotek MT-29B Microporous Insulating Board
MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T..