Polymer Property : Compressive Strength = 13000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 89.7 - 91.4 MPa
13000 - 13300 psi
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphit..
Compressive Strength 89.6 MPa
13000 psi
10% Def.; ASTM D695
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet)
Compressive Strength 89.6 MPa
13000 psi
10% Def.; ASTM D695
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet)
Compressive Strength 89.6 - 110 MPa
13000 - 16000 psi
ASTM D695
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Compressive Strength 89.6 - 103 MPa
13000 - 15000 psi
ASTM D695
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound
A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Techmer ES Plaslube® NY-1/SI/2 WT PA66
Compressive Strength 89.6 MPa
13000 psi
parallel to thickness
Zircar Refractory Composites RS-200 Refractory Sheet
ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Compressive Strength 89.6 MPa
13000 psi
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive
TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting..
Compressive Strength 89.6 MPa
13000 psi
parallel to thickness
Zircar Refractory Composites RS-201 Refractory Sheet
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Compressive Strength 89.6 MPa
13000 psi
parallel to thickness
Zircar Refractory Composites RS-202 Refractory Sheet
ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit..
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Chesterton ARC 10 Paste grade machinable composite
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag..
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m..
Compressive Strength 89.6 MPa
13000 psi
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer
Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell..
Compressive Strength 89.6 MPa
13000 psi
uncured
Atom Adhesives AA-CARB 61 Epoxy Adhesive
AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me..
Compressive Strength 89.6 MPa
13000 psi
Ultimate; TM R050-38
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Chesterton MRS 10 Metal Rebuilding System
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10..
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Chesterton MRS 58 Metal Rebuilding System
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo..
Compressive Strength 89.6 MPa
13000 psi
10% Def.; ASTM D695
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet)
Compressive Strength >= 89.6 MPa
>= 13000 psi
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures
Description: Master Bond Supreme 10HTND-3 features a blend of performance properties including both high shear and peel strengths along with a totally non-drip application feature. This one componen..