Compressive Strength 70.0 - 90.0 MPa
10200 - 13100 psi
ISO 604
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Compressive Strength 70.0 - 90.0 MPa
10200 - 13100 psi
ISO 604
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..