Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Tensile Strength | 93.1 MPa | 13500 psi | LW; ASTM D638 |
Haysite H1000 Polyester Laminate Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide.. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 109 L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Copolymer and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Teknor Apex Chemlon® 217 GI Nylon 6, 17% Glass Fiber Reinforced Features: High Impact, 17% Glass Reinforced; Highly toughened compound designed to improve practical toughness and ductility Processing Method: Injection Molding Forms: Pellets Additive: Impact Mod.. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 93.1 MPa | 13500 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFABS 4030 Glass Filled Acrylonitrile-Butadiene Styrene AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |