Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 9010 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 62.1 MPa
9010 psi
ASTM D412
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection ..
Tensile Strength 62.1 MPa
9010 psi
ASTM D412
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and..
Tensile Strength 62.1 MPa
9010 psi
ASTM D412
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..
Tensile Strength 62.1 MPa

@Temperature 23.0 °C,
Time 0.000 sec
9010 psi

@Temperature 73.4 °F,
Time 0.000 hour
Thirty mil sheet immersion
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..
Copyright © lookpolymers.com All Rights Reserved