Polymer Property : Tensile Strength = 8110 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 55.9 MPa
8110 psi
ASTM D412
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon.
Tensile Strength >= 55.9 MPa
>= 8110 psi
ASTM D 638
Karina E 830-10/145-A-ERYB-LMP White PVC Compound
Heavy metal free PVC compound recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C...
Tensile Strength 55.9 MPa
8110 psi
ASTM D638
Gromax CCP PBT 1100-104S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Tensile Strength 55.9 MPa
8110 psi
ASTM D638
Samyang Tribit® 1500A15 PBT, Inorganic Reinforced
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500A15 contains inorganic filler.Applicati..