Samyang Tribit® 1500A15 PBT, Inorganic Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Samyang
Trade Name Tribit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tribit® 1500A15 PBT, Inorganic Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500A15 contains inorganic filler.Applications: Automotive Bezel - for thermal resistance and direct depositionInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 55.9 MPa
8110 psi
ASTM D638
Elongation at Break <= 10 %
<= 10 %
ASTM D638
Flexural Yield Strength 95.1 MPa
13800 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm

@Thickness 3.17 mm
0.735 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 197 °C
387 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648