Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.9 MPa | 8110 psi | ASTM D412 |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | >= 55.9 MPa | >= 8110 psi | ASTM D 638 |
Karina E 830-10/145-A-ERYB-LMP White PVC Compound Heavy metal free PVC compound recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C... |
|||
Tensile Strength | 55.9 MPa | 8110 psi | ASTM D638 |
Gromax CCP PBT 1100-104S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 55.9 MPa | 8110 psi | ASTM D638 |
Samyang Tribit® 1500A15 PBT, Inorganic Reinforced Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500A15 contains inorganic filler.Applicati.. |