Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.101 MPa | 1175 psi | ASTM D412 |
Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag Reversion Resistant Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the producti.. |