Polymer Property : Tensile Strength = 1175 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.101 MPa
1175 psi
ASTM D412
Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag
Reversion Resistant Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the producti..