P & P Technology Silicone Sheet

Category Polymer , Thermoset , Silicone
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology Silicone Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone sheet is FDA approved. Translucent sheet is FDA @ WRC approved. FDA Certificate No. 177.2600Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Solid Silicone Rubber Sheet
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Solid Silicone Rubber Sheet
Tensile Strength 5.50 MPa
798 psi
Solid Silicone Rubber Sheet
Elongation at Break 450 %
450 %
Solid Silicone Rubber Sheet
Compressive Strength 0.0700 - 0.110 MPa

@Strain 40.0 %
10.2 - 16.0 psi

@Strain 40.0 %
Sponge Silicone Rubber Sheet
Compression Set 6.0 %

@Temperature 150 °C,
Time 252000 sec
6.0 %

@Temperature 302 °F,
Time 70.0 hour
Sponge Silicone Rubber Sheet
25 %

@Temperature 150 °C,
Time 252000 sec
25 %

@Temperature 302 °F,
Time 70.0 hour
Solid Silicone Rubber Sheet
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Solid Silicone Rubber Sheet
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Solid Silicone Rubber Sheet