Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 517 - 703 MPa | 75000 - 102000 psi | |
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |